OH, OH,,,,be carefull on this one. I needed to ease the assy of PGA's also and found some material which was advertised to do the job. However, it cost a fortune to repair the damage done. Tried something else and the same problems of opens, etc....what I am recommending is not to use anything. It may work for a while and make the job easier, but you will pay for this down the road. Wonder what other people will say. *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************