HADCO recommends a remaining material thickness of .012" (+/-.002") for .062" thick boards. The tolerance precludes scoring simultaneously with two blades. Thirty degree cutters are standard, and remove less material than a wider blade. Establish a minimum metal keep-out zone of .025" adjacent to score line. Scoring offers these advantages: Ease of separation Possible increased panel utilization Eliminates solder splash during assembly Smoother finished edge Cost for score or rout is a wash, but a combination of both may add cost to your design. Parts must be rectangular, and breaking corners is not possible. Tom Coyle Field Services Engineer HADCO Corporation On 0.062 inch thick boards, we currently call for a 30 degree score, 0.020 inch deep on opposing sides of the board. We are trying to develop our standard for scoring. Is this what most use for scoring? Do you score boards thicker than 0.062 and if so what dimensioning do you use for those? If given the choice would you select scoring over routing? why? Thought this might be of general interest to the board community. ************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************