Also, have you performed microsections (cross sections) to determine what kind of material is at the core of the nodule? Small nodules usually require at least a few tries to get the small core. Be patient. Matt Byrne Hadco-Owego ______________________________ Reply Separator _________________________________ Subject: Re: COPPER PLATING:Tiny nodules in plated through holes Author: [log in to unmask] at SMTPLINK-HADCO Date: 5/22/97 01:21 AM Mr. Khan, Your problem would be difficult to address without additional details, some questions and possible items to investigate are as follows: How large/small are the nodules, and what sort of problem do they create for the use or sale of the boards? Are they found in the holes only, or are they also on the surface? Are they found in all hole sizes? Are they found in all areas of the panels? Is the problem constant or intermittent? Have you tried a bright nickel flash to help make possible nodules in the chemical copper more easily seen? Lack of reflectivity can make them hard to see. You didn't mention the filtration on the electrolytic copper. Particles in the electrolytic copper bath would be a prime suspect. The removal of small particulates would require a large area of very fine (1 micron or less) filters. You mentioned control of the additive in the electrolytic copper by amp hour, have you confirmed that the proper concentration is present via Hull cells, CVS, and/or HPLC? High additive concentration, organic contaminants, high temperature, and/or high copper concentration in the electrolytic copper bath can contribute to dullness or lack of leveling in the lower current density areas (e.g. in the holes). To test for low current density problems, try plating in the Hull cell (air agitated) at 1 amp for 30 min. Low current density problems are more easily seen in the Hull cell with the longer plating time. If the problem is related to poor low current density performance of the electrolytic copper, raising the current density (e.g. 3 amps/sq dm) may provide a temporary fix. If this helps, the items above should be investigated. Please feel free to contact me directly for more detailed discussions. Regards, Paul Galatis Electrochemicals E-mail: [log in to unmask] *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************