There are many reasons for both the board and the PBGA to warp during reflow, and some degree of warpage in PBGA may not be avoidable. Typically, the differences in CTE of materials and cure shrinkage of the encapsulant are the main causes of package warpage. Please keep in mind that the following factors can have direct impact on the coplanarity of PBGA. - PBGA substrate >Thickness >Material (BT/FR-4) - Encapsulation Material (Glob top vs Molded Top) - Thermal Profile during reflow - Si Die size Hope this helps, Michael Yuen ---------- From: TechNet-request To: technet Subject: PBGA warpage (assy) Date: Thursday, May 22, 1997 1:16PM I recently had some PBGA's reflowed using a hot air rework station. All of the PBGA's warped. What could be the cause of the warpage? Regards, Geoff Horrocks Manufacturing Technology Group Fitel-PMX 24 Colonnade Road Nepean, Ontario K2E 7J6 Phone: 613-723-8939 Fax: 613-723-8349 *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************