We're currently using Kester R244 and if anybody out there has used this paste, please share with me your experience with this paste and how it performs when it has been stored at relatively "extreme" temperatures, such as -20C and 10C. We are currently storing ours at 4C and we would like to determine what our storage tolerances should be. We are looking at a window between -10C and 10C. Also, has anybody used this paste after it has been stored at around 8 hours at approximately dry ice temperature? What do you suppose would happen after paste stored at this cold temperature is reflowed? Regards, Siegfried Quemado [log in to unmask] *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************