351S was tested for Bellcore SIR at a different time than the pealable mask study was made. 4 day geometric means (ohms) 351S comb down 2.5E12 351S comb up 2.4E12 Controls 2.0E12 351S is a fairly benign low residue flux, and Bellcore compliant. *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************