Dennis, You can probably get away with only calibrating features of the machine that are "adjustable" which might not include e.g. air velocity, but I would recommend a calibration strategy based on actual product temperature for the following reason: Reflow is a non-eqilibrium process so the product temperature is dependant on belt speed and air flow velocities as well as zone temperatures so, for an oven controller based calibration, all of these parameters should be calibrated. Increases in surface emmisivities (due to flux build up or oxidation) could also affect product temperature by increasing IR heat transfer (although I have no evidence for this). If you use a KIC system then again you are not checking the actual product temperature. A Datapaq or Mole system will give you actual product temperature and can easily be sent away for calibration once a year. Another option that we have developed in partnership with Quad, and which has just become available, is to use an oven equipped with a line scanning infra-red sensor (which can again be calibrated to the required standards) and which will monitor actual product temperature board after board. (As this is a new concept in reflow process monitoring I hope I will be forgiven what may sound like advertising.) David Whalley Manufacturing Engineering Department Loughborough University Loughborough Leics LE11 3TU UK Tel. +44(0)1509 222930 Fax. +44(0)1509 267725 [log in to unmask] http://info.lboro.ac.uk/departments/en/STAFF/David_Whalley/index.html At 12:22 24/03/97 -0500, you wrote: >I need to calibrate a conveyerized IR oven used for tin/lead reflow. The >calibration must comply with ISO and military calibration standards. Until >now we have been using an outside source to calibrate the oven. I was not >satisfied with the method they used. I was wondering if other organizations >are using reflow profiles, or physical calibration of the oven controls to >meet military ans iso requirments. > >Thank you for your replies > >Dennis > *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************