In message "D. Rooke" <[log in to unmask]> writes >In the same vein, are there any Cupric etchers out there using sodium >chlorate as the oxidant as opposed to hydrogen peroxide? Again, any >positive/negative impacts? I was recently looking at the pros and cons of using sodium chlorate as a more stable oxidiser as we currently use hydrogen peroxide. I think the sodium chloride you spoke of is just the by-product of the reaction with sodium chlorate and not an additive system in its own right. When I queried the change with our disposal company, they advised that they would not be able accept the etch if it contained sodium chloride. They currently take our spent etch away and plate out the copper for which we receive a credit. Hope this helps, -- Paul Gould *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************