Hi, I never did .. But I have tried running a QFP-208 and PLCC68 without dropping the component during double sided reflow.. Poh.. --------------------------------------------------------------------------- At 08:05 AM 4/3/97 EST, you wrote: > Hello, > > Does anyone calculate the max chip's weight for double side reflow in > > more accurate way then comparing the surface tension with the gravity > > force. > > Thanks, Tamir > >*************************************************************************** >* TechNet mail list is provided as a service by IPC using SmartList v3.05 * >*************************************************************************** >* To subscribe/unsubscribe send a message <to: [log in to unmask]> * >* with <subject: subscribe/unsubscribe> and no text in the body. * >*************************************************************************** >* If you are having a problem with the IPC TechNet forum please contact * >* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * >*************************************************************************** > > *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************