Doreen, When the lead and solder joint leave the pad under this lateral force, could it be that the CuSn intermetallic has been fractured? Might want to check that out. Dennis Mitchell Zycon ______________________________ Reply Separator _________________________________ Subject: "Rubber" Solder Author: [log in to unmask] at corp Date: 4/14/97 12:32 PM I have heard reports from a lab technician indicating that he has seen "rubber" solder joints on some boards we had built. The boards had an organic coating before soldering. I saw the condition myself, but have to admit that I am not accustomed to poking at solder joints; I usually just observe them. In six years of surface mount experience, I have never seen this condition, nor have I heard of it. The condition is explained as follows: Using a relatively blunt object (e.g. not a probe or pick), the component lead can be moved within the solder joint without visible fracture to that joint, and without the joint moving off the pad. The force used is undetermined, but I would consider it relatively gentle, less than the magnitude of force used when trying to pull a lead out of a joint. In some rare cases, the lead slides completely off the pad with the joint still perfectly attached. I think this indicates a problem with the surface finish. In addition, some joints are very malleable; by using a blunt object, it is easy to dent a joint without visible fracture. My questions are: * Has anyone else ever seen this phenomenon? * Does anyone venture to guess the root cause, or if this might be an illusion? Doreen Fisher Dell Computer Corp. [log in to unmask] *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************