From: Charles Orchard Subject: (U) DES: Solder Reliability Software Hello, I recently had the opportunity to evaluate the solder reliability software from EPSI Inc. (a technical description of the capabilities of the software with examples is in the Conference Proceedings from SMI 199 pg 136-151). What other commercially available solder reliability software is out there? Has anyone performed any comparisons? The author compares to Norris-Landzberg, Engelmaier/IPC, Darveax (Motorola), CSMR(AT&T), and HIPADIC-P(Hitachi). Charles Orchard - Quality Engineering (SSD Products) Tie 8-778-6305 Page (416) 330-8898 *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************