Hi TechNet - The IPC Microsectioning committee put out a poster that contains several common board defects in a cross sectional view. Contact Mike Buetow at IPC for more info. Dave Hillman Rockwell Collins [log in to unmask] ______________________________ Reply Separator _________________________________ Subject: Cross Section Defects Author: [log in to unmask] at ccmgw1 Date: 4/28/97 2:28 PM Many years back DEC had posters of some common defects found in cross section. My technicians have been asking if there are any newer posters available in the industry? I have contacted Struers and they do not believe they have any or know of any available. Any suggestions? *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************