Bob Common sense :-) Fit, Function, and Reliability should be your guidance. Insure that the wire will not snag or break from stress and material fatigue during normal handling and use in the product. Support within 1 inch of the connection, to strain relief the solder joint, is a good minimum to start with. ______________________________ Reply Separator _________________________________ Subject: assembly-jumper wires Author: [log in to unmask] at CCGATE Date: 4/28/97 11:21 AM To whom... 28 Apr 97 If I have wire jumpers on a mulitlayer pwb, is there a standard that defines the distance between bond points on the wire length. I know that Mil-Std-275 and IPC-2221 both call out bonding at 1" intervals, but I am looking at test set equipement, not hi-rel avionics hardware and IMO the 1" interval is an overkill. Is there any guidence, good commercial standard, out there or if not, what is being done? Thanks in advance. Regards, Bob Vanech Bob Norden Systems (203) 852-4810 *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************