Hello, Does anyone have any experience with removing a high-density (>100-pins) PTH connector that is both press-fit and soldered (not my design)? So far, I came up with preheat/prebake @ 250 F for 1-4 hrs and use a solder pot (i.e., Air-Vac), but I'm worried that I will damage the through holes. Regards, [log in to unmask] *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************