Technetters: I am soliciting opinions on conformal coating of PBW-mounted connectors. Our manufacturing folks refuse to conformal coat within 1/8" of any board mount connectors. They contend the conformal coating will wick up the pins and get on the contact areas, regardless of the type of conformal coating used or the method of application. The connectors are not sealed. These boards have to pass salt fog & humidity testing and I don't like the idea of having bare areas, especially at the interface where the connector meets the board. Does anyone have any experience with this? Thanks in advance for your help! S. Smith, Tracor Aerospace Electronics Systems *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************