Tom, I will be very interested in reading it. Please send me one @ Attn: Yuan Li, 1685 38th St., Boulder, CO 80301. Thanks, Yuan ______________________________ Reply Separator _________________________________ Subject: Re: OSP versus HASL Author: [log in to unmask] at UNIXMAIL Date: 3/4/97 10:49 AM Enthone-OMI has compiled a booklet of non-biased "industry written" technical papers which would answer your questions. One such paper was written by K. Banerji from Motorola entitled "HASL Free Finishes From An Assemblers' Viewpoint". In it he discusses solderability test results of surface finishes such as HASL, OSP and ENi/IAu. He also details his findings regarding solder joint reliability and processing issues. Should anyone be interested in a (free) copy, please contact either Eric Stafstrom at (203) 932-8633 or myself and we would be happy to forward one your way. Tom Eshelman [log in to unmask] (800) 548-9801 ext. 7257 *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************