I am soldering J-leaded and gull-wing SM components with high temperature solder and find that the tin/lead solder coating on the components interfere with the integrity of the solder joint. The retinning process and pot to pot dipping is only partially successful and considerable amount of the tin-lead solder is retained in the joints, also many of the components are not availble with other final finishes. I was going to use a tin-lead stripper, but some of my colleagues have had problems with possible leakage and later failure of the components. Component bodies are both ceramic and plastic. Any suggestions. Phil Hinton [log in to unmask] 520-745-1013 *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************