There is numerous literature on this subject. Agood starting point with reference is the book, "Solder Joint Reliability" edited by John H. Lau Nick Biunno Zycon Corp. ______________________________ Reply Separator _________________________________ Subject: Mechanical Properties: Intermetallic Thickness! Author: [log in to unmask] at corp Date: 3/21/97 10:22 AM Related question on mechanical properties! Are there any publications out there documenting the adverse impact(s) of excessive intermetalic growth of Eutectic Solder (Not Gold Embrittlement just regular Cu3Sn and Cu6Sn5)? Thanks *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************