Your problem is likely not the Pd-Ag surface layers, but the underlying metal to which you need to wet. Either that base metal is contaminated and thus poorly wettable or it may be made of a material, e.g. Alloy 42 (check with magnet), that is inherently difficult to wet. Werner Engelmaier Engelmaier Associates, Inc. Electronic Packaging, Interconnection and Reliability Consulting 23 Gunther Street Mendham, NJ 07945 USA Phone & Fax: 201-543-2747 E-mail: [log in to unmask] *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************