Subject: ASSY: Re: Flexible Circuit Repair -------------------------------------------------------------------------------- Common polyimide flex materials are rated for soldering at 550F or 500F max., depending on the type of adhesive. Andy Magee - Applications Engineer Rogers - Circuit Materials Tel: (602) 917-5237 Fax: (602) 917-5256 E-Mail: [log in to unmask] Website: http//www.rogers-corp.com/cmu //////////////////////////// // SERVICE TO THE LINE, // // ON THE LINE, // // ON TIME. // //////////////////////////// ______________________________ Reply Separator _________________________________ Subject: Flexible Circuit Repair Author: Tracey Spencer::(SPNCRTAA) at ~FABRIK Date: 2/4/97 11:52 AM From: Tracey Spencer Date: Tue, Feb 4, 1997 11:52 AM Subject: Flexible Circuit Repair To: Andrew P Magee; TechNet What is the maximum allowable tip temp for soldering/de-soldering of components, both through hole and surface mount, to flexible circuits? ---------------------------- Forwarded with Changes --------------------------- From: /S=cc:Mail-Gateway/OU2=XSFCC/OU=ZWGBA/P=MOT/A=MOT/C=US/::(SCCMLGAB) at ~FABRIK Date: 2/5/97 6:58PM -0800 To: Andrew P Magee at Rogers-MCD Subject: Message Undeliverable to cc:Mail ------------------------------------------------------------------------------- *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************