Hi Victor - The use of a low temperature solder alloy will depend on what use environment you are putting your product into. An example - there is a bunch of data that shows that Sn/Pb/Bi alloys that are used above 100C are not reliable because of a eutectic melting point that Sn/Pb/Bi forms at 98C. Many people use low temp alloys very successfully. Contact your solder suppliers for information on their low temp alloys and possible applications. Dave Hillman Rockwell Collins [log in to unmask] ______________________________ Reply Separator _________________________________ Subject: Low temperature solder Author: [log in to unmask] at ccmgw1 Date: 2/2/97 9:15 PM Hi, I am looking for info. or prices of the low temperature solder pastes? Are these solder pastes used in shop floor at all? What is your opinion in using this ? Thank you very much. Best regards, Victor *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************