Please send this back to the person concerned about SR coat contaminating nearby soldering processes: We've been spraying SR coating in a Nordson Select Coat machine for a couple of years, and while we don't exhibit silicone buildup on nearby work surfaces, we do have slick floors in the area around the machine, probably due to walkoff from the machine operators. Our machine's exhaust is routed through a charcoal filter and vented at ceiling height above the machine, so it's possible we lose some silicone through the filters into the surrounding area, but not much. Benjamin A Guthrie Phone: (219)429-8324 >Mail Stop:15-23 Fax: (219)429-4688 Email: [log in to unmask] >MESC, 1313 Production Road, Fort Wayne, IN 46808 I sent this up to the server last week, but can't find that I ever got a >>>"come-back" copy, so here goes again. >>> >>>Following is posted for one of our clients: >>> >>>"I have a vendor that has installed a closed system conformal coat spray >>>machine in the middle of an area where surface mount and through hole >>>processing occurs. The coating being used is silicone based. I'm >>>concerned about silicone contamination of other materials in the work area, >>>due to unintentional migration (overspray in the atmosphere, fumes/gasses >>>from curing process, etc.) over time, that could affect the soldering >>>processes. Are there any specifications or guidelines for SR coating >>>controls in a printed circuit board assembly house? Is this a valid >>>concern? Does anyone have a good or bad history of a similar situation?" >>> >>>Thanks for inputs anyone has. Jack >>> >>>***ALL NEW EMPF PHONE NUMBERS*** >>> >>>Jack Crawford, HelpLine Coordinator >>>Electronics Mfg. Productivity Facility >>>****NEW--317.655.3688 >>>****FAX 317-655-3699 >>>714 N Senate Ave, Suite 100 >>>Indianapolis IN 46202-3112 >>>VISIT OUR HOME PAGE AT: http://www.empf.org >>>[log in to unmask] >>>-------------------------------------- > > > > ---------------------------------- Jeffery L. Hempton Phone: (219) 429-7335 Fax: (219) 429-4688 Boardshop Manufacturing Engineer Mail Stop: 25-31 Hughes Defense Communications 1010 Production Road, Fort Wayne, IN 46808-4106 Email: [log in to unmask] "Those who dream by day are cognizant of many things which escape those who dream only by night" - -Edgar Allen Poe *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************