I have not experienced the resin beads but it is good to keep in mind for future reference. A good filtration system should capture most anything suspended in solution. The main problem with most plating tank filtration systems is there's really no way to "suck" up everything off the tank floor. Any disturbance reaching the bottom will kick up debris which may eventually end up on the PCB. A general rule is about 3 turnovers per hour. DNHJR ______________________________ Reply Separator _________________________________ Subject: Plating Particulates Author: [log in to unmask] at corp Date: 2/7/97 4:53 AM Suppose you're plating in an acid copper bath and notice particles from vacuum filtration in the lab. You then arrive at the conclusion these are resin beads that have fragmented out of the DI unit. What are the ramifications? Has anyone seen this? Can they be filtered by bath recirculation? What is the normal turnover (recirculation) time in an acid copper bath? Thank you in advance, Chemist [log in to unmask] [log in to unmask] *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************