I have several questions regarding the shelf life as follows : 1) What is the shelf life of HASL boards & OSP boards ? SIX MONTHS. 2) Are the shelf life requirements documented anywhere ? I THINK IPC 276 LISTS THE SHELF LIFE AND SO DOES THE WEAPONS SPEC 9858. I CAN'T REMEMBER IF THE LAST TWO NUMBERS (58) IS CORRECT. 3) If not, what is the acceptable practice (as in good industry practice) in the industry ? INDUSTRY STANDARD IS SIX MONTHS. CRAIG KURTZ HI CRAIG: CAN YOU PROVIDE SOME ANSWERS TO THE QUESTIONS BELOW?? THANKS GLENN ______________________________ Forward Header __________________________________ Subject: Tech ? from Lucent Author: Rich Chenoweth at C3-MAILROOM Date: 2/26/97 11:19 AM Lee/Glenn, Questions as forwarded from technet ______________________________ Forward Header __________________________________ Subject: Shelf Life Author: [log in to unmask] at INTERNET Date: 2/26/97 10:52 AM Hello TechNetters, I have several questions regarding the shelf life as follows : 1) What is the shelf life of HASL boards & OSP boards ? 2) Are the shelf life requirements documented anywhere ? 3) If not, what is the acceptable practice (as in good industry practice) in the industry ? I would appreciate responses regarding this matter. Thanks in advance, Mukesh Dave [log in to unmask] *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************