X400-Mts-Identifier: [ /P=MOT/A=MOT/C=US/ ; c\sbnc3\970219190853b ] X-Mailer: Worldtalk (4.0.2-p15)/STREAM Resent-Message-ID: <"yGKZS2.0.Q18.fqj2p"@ipc> Resent-From: [log in to unmask] X-Mailing-List: <[log in to unmask]> archive/latest/10359 X-Loop: [log in to unmask] Precedence: list Resent-Sender: [log in to unmask] Thanks for details explaination on Sn+2 AND Sn+4 Oxidation. This is reffering to Plating solution discoloration. We manage control this using Solderon RD by Lea Ronal or Hydroquinone in Technic system. I was reffering to discoloration on the "work/lead frame". The leadframe is copper. Thus we plating solder (tin + lead) over copper. My problem is; When the plating machine stop immediately the partially plated leadframe will change to gray or dark color. When the production resume this gray/dark color remain on the leadframe. Some time this portion will fail solderability test (fail to mount to PCB). Somebody told me that this is due to Methane Sulfonic Acid remain on the leadframe and oxidise the leadframe. I tried to rinse the leadframe everytime the production stops. Slightly better but not good enough. What is actually the grey/dark color on top of solder layer? Any other suggestion to solve this problem? _______________________________________________________________________________ Subject: Re: Discoloration in solder plating From: [log in to unmask]@INTERNET at #EMAIL Date: 2/17/97 12:01 PM Misri Mohd replied to me personally that they are using the Methane Sulfonic Acid based electrolyte. The Methane Sulfonic Acid based system has certain properties that must be attended to when plating Tin or its alloys that may be causing some of the problems alluded to in the previous message. Tin has two oxidation states besides the metal, Stannous ( 2+) and Stannic (4+). The Stannous Tin, which is the normal, and preferred, state in this bath, readily oxidizes to Stannic Tin in the presence of either atmospheric Oxygen, or if the anode area is too small for the current being pushed through the bath. When Stannic Tin forms, it is insoluble, and forms a milky looking precipitate in the bath. The Methane Sulfonic Acid bath is clear, (not to say uncolored) when there are is no Stannic Tin in the bath. This milky precipitate normally stays suspended in the bath, and can plate out, (co-deposit) and become part of the plating. The amount of the Stannic Tin plated out will change with the current density, with greater current density tending to plate more Stannic Tin. This could be the cause of some of the color change of the plating. The Stannic Tin is difficult to filter out, but there are ways to get it out of the bath, and my guess is that there are people reading this that can give this gentleman some directions at finding the appropriate technology. Alternately the plating bath supplier may be able to assist in this matter. Hope this helps Rudy Sedlak RD Chemical Company *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************