During the IPC conference in San Jose, a paper entitled "BACTERIAL CONTAMINATION OF CHEMISTRY USED IN PWB MANUFACTURING" will be presented. Jill Steeper of Shipley will give this paper on 3/11/97 at 1:30p. Included in this paper are types of bacteria, process areas most commonly affected, problem resolution, and monitoring mechanisms. The Shipley Company John S. Grosso Director PWB Research, Development, & Engineering (508)229-7441 *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************