Based on years of experience with aqueous dry film solder masks, may I offer some bits of information regarding ionic cleanliness with these kinds of products. 1. You will never be able to achieve readings with dry film solder masks (DFSM) as good as you can get with the LPI solder masks. They are thicker, more porous and they are all one component materials (you can't make a two component DFSM). Therefore, DFSM's tend to be less reactive and don't crosslink as much and ionic components tend to "leach out" during the testing. 2. The ionic cleanliness testers that used heated/agitated solutions (such as the Omegameter 600 SMD) tend to give readings that are much worse with DFSM's than the non heated testers. 3. You can achieve ionic cleanliness readings that will meet common specs (<10.0 micrograms/square inch for the MIL-P-55110C and <6.45 micrograms/square inch for the Bellcore spec); however getting much better than this is diffucult. Even reaching these levels with DFSM's in no "cake walk" and may require: A. A UV cure step during the processing of the mask at the PWB fab site. B. Care that the boards are not subjected to harsh processes (such as hot air leveling for multiple passes) after the mask has been fully cured. C. If aqueous fluxes are used at assembly and saponifiers are used in the post clean it is a good idea to have a good DI water rinse after the tap water rinse to get the mask as clean as possible. A quick bake (say 10 min at 250 deg F) after post clean and prior to ionic cleanliness testing also helps. Good luck and please contact me if you'd like additional information. Larry Fisher Dexter Electronic Materials 317-628-7401 [log in to unmask] *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************