A surface coating of oil on the solder pot reduces dross formation. This sits on the top of the pumping zone. The product comes in solid form and melts at higher temperatures. I'm sorry I can't remember the details but will find out Monday. Paul Gould *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************