Remember...IPC-RB-276 is OBSOLETE! IPC-6011 and IPC-6012 are the bad boys now unless your vendor isn't up to the new ones yet. Dan Lorinser BFGoodrich Aerospace >>> George Franck Jr <[log in to unmask]> Jan 21, 1997 1:19 pm >>> Technet, If you are a Fab Shop, or if you know of a good one, please pass this along. I currently have requirements for Copper Invar Copper (CIC) boards. Looking for one or two shops to quote. Not big volume (3500 boards square inches total). Boards USED TO BE Mil-P-55110, but will be built to IPC-RB-276, Class 3, INCLUDING COUPONS. We can negotiate details. Boards are 5 layer boards. Some designs have blind vias 1-2 and 4-5. er...one more thing.. Polyamide, GIN/GIL per 13949. E-mail which suggest better/cheaper ways to build these boards will be read with interest, however where were you in 1989 when we design it the first time? Send me an E-mail or Call. George Franck Raytheon E-Systems (Texas Instruments / Hughes) Falls Church Virginia 703 560 5000 ext 2648. "When you expect the impossible, it might get designed that way" -- George Franck Jr Raytheon E-Systems Falls Church Va. "The opinions expressed are those of the author, and are not necessarily those of the Raytheon Corporation." *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************