Questions you need to answer: 1. Are there keep out zones? 2. What is 100% moisture resistance? (hint, it does not exist) 3. What environment must the board survive? The simplest method is to tape off the the keep out zones and hand spray. Thickness control is lost, but you can coat the boards. Humiseal, Dymax, and Dow all have good coatings, with their various +'s and -'s. ______________________________ Reply Separator _________________________________ Subject: conformal coating help Author: [log in to unmask] at Internet Date: 1/21/97 8:56 AM We need to provide 100% moisture seal on the top surface of some FR-4 boards about 8"x12" that have SMT components mounted. Can I do this "easily" in-house without much equipment? What materials and suppliers? We could easily install a fume hood if necessary. This is not a high volume project. What do I do about sealing vias? thanks, Crawford Byxbee *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************