I'm looking for any cautions or advice you may have on the following. We are considering the use of immersion tin as a finish on bare printed circuit boards. The boards are thru-hole only and they will be wave soldered within the next 3-4 weeks. Do you consider this a "no no" or is this an acceptable finish until wave soldering? *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************