Fellow Technetters: What is the "rule" regarding lifted pads on multilayer boards? We have always scrapped them. A subcontractor recently returned a few of our boards which had lifted pads. We follow IPC-A-610B class II. The subject is not mentioned. Comments are appreciated. Ellen Berkman Excalibur Systems *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************