this is "Epoxide cellulose paper core, epoxide glass cloth surfaces copper-clad laminated sheet of defined flammability (vertical burn test)." - the title of the IEC 249-2-9 specification. FV 0 is the flammability rating which appears equivalent to UL 94V-0. ______________________________ Reply Separator _________________________________ Subject: IEC 249-2-9-FVO-EP-CP Author: [log in to unmask] at smtplink Date: 1/10/97 1:16 PM Can anyone tell me what this material (IEC 249-2-9-FVO-EP-CP) is? Is it FR4, CEM1 etc Thanks. Tom Killick CIT 510 829 0154 *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************