We can train an operator who never ran a machine or hand soldered in a couple of weeks to run a wave or a few days for hand soldering using no clean soldering on simple panels. High density, poorly designed panels, old panels...etc, the operator can be up an running fast, but operators with little experience will produce very poor yield, experienced operators can produce "good" yield in spite of the problems. The big problem with conversion is not operator training, it is machine set-up, panel profiling and product design. These are all controlled by engineering, not by operator training. As for military acceptance criteria, it depends on the operator how fast they accept change, which varies operator to operator, and how much support change has from production supervision. ______________________________ Reply Separator _________________________________ Subject: Time to train operators: J-STD-001 and LRNC flux Author: [log in to unmask] at internet Date: 1/7/97 6:19 PM Technetters: I'd be interested to hear how long it takes to train an operator (who is used to working to military soldering standards) the operator- related parts of J-STD-001 (i.e., acceptance requirements). I'd also like to hear how long it takes to train an operator (who is used to working with RMA flux) to solder using a low-residue no-clean flux. Gordon Davy *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************