Chad: I would suggest calling Bob Burris at SEHO. He is very knowledgeable on reflow ovens. Bob can be reached at 804-798-6000, SEHO USA Inc., in Ashland, Virginia. Ron Hollandsworth [log in to unmask] ______________________________ Reply Separator _________________________________ Subject: convection rates Author: [log in to unmask] at INTERNET Date: 1/31/97 3:29 PM I am interested in talking with someone about measuring convection rates in reflow ovens. Thanks, Chad Jones *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************