We do not have a problem with slivers when using 1/2oz foil. However we do have one customer who uses an ultra sonic cleaning process during assembly. This created some slivering. We have gone to 1/4oz material on outer layers for that customer. Kim ______________________________ Reply Separator _________________________________ Subject: Gold as Etch Resist Author: [log in to unmask] at SMTPLINK-HADCO Date: 1/29/97 9:17 PM Hello, Please post information, experiences, and anecdotes, on using electroplated gold as an etch resist. In particular how is the etch rate controlled. How can the undercut be reduced to eliminate the chance of slivers. (Gold/Nickel/Copper/FR4 :The copper gets etched) Thanks Rich *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************