Hi Werner, To clarify a point on the SOT23 leadframe alloy. All SOT23 packages are not necessarily Alloy 42. Historically, eutectic die attach was used, for which A42 was the preferred material. More recently, copper alloys are being used, with epoxy die attach, primarily for their improved thermal conductivity. The end user who is more concerned about the alloy composition, can easily check whether it is an A42 or Cu alloy by taking a unit, snipping a lead and looking at the cross-section. If its a copper colour guess what, - its copper, if its a silver colour its A42. Just be careful to use a decent pair of snips as otherwise you may smear the solder plating over the cross section and assume a copper alloy is A42, as the smeared solder plating will give a silver appearance. regards, Olly Kierse Analog Devices BV *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************