Hi Gordon! Dr. Tench and others have done additional work that furthers the information you mentioned in Klein Wassink's book. SnO2 does form at room temperatures. Think of it this way - a layer of SnO forms on a new solder surface, once it gets thick enough that the Sn has a long diffusion path the outer surface begins to convert to SnO2 because of the abundance of O2 in the air. This SnO2 layer never gets very thick but because it is the stable form of Sn oxide - it is very coherent and very insulating. The insulative nature of the oxide and its structure make it hard for fluxes to effectively remove it. A couple of references with a bunch more detail are: "The Mechanics of Solder Alloy Wetting and Spreading, ISBN 0-442-01752-9, chapter 6 Oxidation of Solder Coatings by Dr. Morgan Tench" " An Examination of Artificially Aged PWB Surfaces Using Sequential Electrochemical Reduction Analysis" by D. Hillman and M. Tench, IPC-TP-1060, October 1992." Your freezer ideas sound strange but I'll try to put some samples in the freezer and do some SERA testing to see what happens - should be fun (oh will the lab techs give me a hard time about this test!). Dave Hillman Rockwell Collins [log in to unmask] ______________________________ Reply Separator _________________________________ Subject: Effects of temp on growth rate of tin oxide and Cu-Sn IMC Author: [log in to unmask] at ccmgw1 Date: 1/17/97 5:28 PM A question has been raised over a couple of the comments I made in a previous TechNet posting regarding the growth of tin oxide on solder and of copper-tin intermetallic compound. I stated that tin (or solder) quickly forms a protective oxide layer a few hundred atomic layers thick, and the growth then effectively stops. While I didn't say so, I was referring to oxidation under ordinary room conditions, not, for example, in an oven or in steam. My basis for making that statement is R. J. Klein Wassink, _Soldering in Electronics_ (2d edition, 1989, p.221, quoting original work by others): Fresh [SnO] layers have a thickness of 1,5 nm and grow approximately _logarithmically_ [emphasis added - not parabolically] with time: at room temperature 2 nm after a week, 3 nm after a year and only 4,5 nm after 20 years (1 nm = 10 angstroms).... The effect of lead (in solid solution in the tin) on the oxidation rate of tin can be neglected.... The tin in the alloy oxidises preferentially, so that for solder alloys the main oxide is SnO, just as for pure tin... I know that Dr. Tench of Rockwell has been studying the oxidation of tin and tin-lead in recent years, and maybe he or someone else has data that conflicts with the above. Perhaps very high relative humidity at room temperature promotes faster or thicker growth. On the other hand, perhaps his findings relate to oxidation at elevated temperature or in steam. I'd be interested to see some data on this question. To the best of my knowledge, the oxide that exists on tin or solder is SnO if it hasn't been exposed to deliberate heating or to steam (in fact, it is this difference that limits the predictive power of steam aging for solderability testing, since steam seems to promote the formation of thick SnO2), but if my info is out of date, please let me know. I also commented about putting a printed board with immersion tin in the freezer. The reason for doing so was not to reduce the rate of oxidation of tin, since that reaction is practically complete before you could get it cold, but to reduce the rate of reaction between tin and copper. (If it is true that SnO slowly converts to SnO2, then freezer storage would potentially be a benefit by reducing the conversion rate. Also, I don't mean to imply that putting boards in a freezer would be economically justifiable, since I don't know whether it is or not, but only to identify what is technically possible.) In general, reaction rates decrease exponentially with decreasing temperature, and the temperature difference between room temperature and a typical home freezer is about 40 deg. C, so that should be enough to reduce the rate of reaction between tin and copper by better than an order of magnitude. (I haven't looked up the activation energy or done the calculation, but I'm sure that this is so.) A commercial freezer gets a lot colder than this, of course, and could be used to reduce the reaction rate by several orders of magnitude. (One order of magnitude would mean that a coating that would preserve solderability for a day at room temperature would preserve it for ten days in cold storage; two orders of magnitude would mean preserving it for a hundred days.) Since my prediction was based not on my experience or anything that I had read, but only on general prinicples, I was encouraged to see the TechNet comment by Robert Welch (who has had a lot of experience - and incidentally, his point about the importance of having the copper be scrupulously clean was well taken, too): And if the project gets hung up for some reason don't fret, just wrap them up like Cristmas leftovers and keepem in the fridge. Finally, I received expressions of concern about the possible harm to a printed board by putting it in a freezer: "condensation, volatiles loss, etc." I can't figure out what the risks are here: 1. Condensation. The condensation would occur when the board was removed from the freezer - frost would form and then melt, but so what? The board spent a lot of time during its fab in solutions a lot more aggressive than a layer of frost or water. 2. Volatiles loss. If a board needs to be stored for a minimum time at room temperature to ensure that volatiles are lost before it is soldered, that's news to me. The only volatile compound that I can think of in a printed board is water. I know that a board can lose - or gain - water during room-temperature storage (depending on how much water it contains to start and the RH of its storage environment). I also know that a board can be baked before soldering to reduce the risk of forming measles (or worse) during soldering, but that would be true regardless of its storage time or temperature. A board would not gain a significant amount of water during freezer storage since the permeation rate would be so low. What am I missing so that I don't perceive a risk? Gordon Davy *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************