What soldermask are you using? ______________________________ Reply Separator _________________________________ Subject: Fab: Finish LPI thickness on circuits Author: [log in to unmask] at corp Date: 1/17/97 1:46 PM We're having difficulties trying to get .001" of LPI solder mask thickness on 2 oz. bare copper circuits. We're screening with a DP-10 using 60 and/or 70 durometer squeegee material. Our screen mesh count has been 86 - 110. We flood - print - print. Any suggestions would be greatly appreciated. *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************