First, please do not send messages TO the list and copy CC to the individual. I will get 2 messages. Thank you. ------------------------------------------------ If your question is [log in to unmask] wrote: > how about pacothane ? I already answer to somebody, but maybe other people are interested: We also use Tedlar, but I believe it is not the best material to be used in such application. I believe that the Tedlar will partially fill the hole (because of the temperature, pressure and vacuum conditions), before the prepeg will have the chance to melt and move through the hole to the surface. For this reasons, the hole looks like a crater, with prepeg flowing outside of the hole, at the edge of the hole, trying to escape the bump created by Tedlar in the hole. As for Pacothane, it does not justify the price, for the results which are almost identical to Tedlar usage. Thanks, Julian We use Tedlar, but I know that this is not the best solution, and I'm looking for something else. I have prepeg outside of the hole; when I look from top of the panel I can see a lot of prepeg around the holes, however looking at an angle (45) I am able to see that the hole is not fully filed (I don't see a bump where the hole is. This is confirmed in the crossection view, even if I cannot see it tridimensional. The difference between the copper surface and the bottom of the hole is probably less than 1 mil, but I don't like it. I use a standard lamination cycle, with kiss cycle, followed by high pressure and heat, under continuous vacuum. Julian *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************