> || Rick Billings | PEMSTAR, Inc | Wrote : > Does anybody have any recommendations on what to try next? Rick, I discussed your problem with our Process Engineer Through-Hole. He came up with the following comment (translated from Dutch): We at Elmo have an Electrovert Centurion 2000S equipped with a so-called Omega Wave. This wave is generated by a vibration-plate in the solder bath, which pushes up the solder for approx. 1/3 of the solder bath length. This stimulates the fillet capability of the solder. With this equipment we don't have problems with fillet height. If you want to know the details, E-mail us, good luck! ********************************** Ivo de Rooij Process Engineer Surface Mount Assembly Fokker Elmo BV (Fokker Aviation) P.O. Box 75 4630 AB Hoogerheide The Netherlands phone (+31)(0) 164 - 6 17 000 fax (+31)(0) 164 - 6 17 700 e-mail [log in to unmask] **********************************