I agree with my friend from Mercury pull testing is a useful test but it can give misleading information if not done correctly. I use it as a method of comparing profile results and the degree of voiding that may be present. It is difficult to directly relate it to reliability data. Bob Willis Electronic Presentation Services 2 Fourth Avenue, Chelmsford, Essex CM1 4HA. England. Tel: (44) 01245 351502 Fax: (44) 01245 496123 Home Page: http://ourworld.compuserve.com/homepages/bwillis Email: [log in to unmask] *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * ***************************************************************************