Good Day All, We are looking for someone who is an expert or knowledgable in the realm of adhesives who would like to consult with us on a project that is giving us some problems. The application is bonding a nickel plated magnet to a PTFE base. If there is anyone interested, please contact: Terry Munson Contamination Studies Laboratories (317) 457-8095. Thanks.