Ron, In response to the attached email: We are currently in the design/prototype stage of a new product that requires selective wave soldering. On the solder side of the pwb there are many high profile devices. The tallest being a 140 pin SMT conn (height off the pwb is 7.5mm) I designed a masking fixture out of a composite material ECP plus 8"L X 8"W X 12mm thick. Because of the tallest component, the solder side of the pwb is 8.9mm from the wave. The fixture creates a type of chimney which the wave must travel up. Preheat didn't seem to be a problem with this fixture probably due to the use of 2 forced convection preheat sections and the last section having IR panels top and bottom. There was no problem getting the solder to go up "the chimney" the problem was the solder flowing out properly. Therefore there was bridging on the leads closest to the exit end of the component. Two changes were made to eliminate the bridging. 1. The pwb and fixture were revised where possible to allow more clearance around the leads to be soldered. 2. The use of an air knife on the wave soldering equipment eliminated bridging in all areas. Based on these tests we purchased an Electrovert Econopak Plus for the production of this new product. Good Luck Dan Shea Sr. Mfg. Engineer The Foxboro Co. Foxboro, MA 02035 [log in to unmask] --- Begin Included Message --- Date: Tue, 04 Jun 96 16:32:16 EST From: "Hollandsworth, Ron" <[log in to unmask]> To: [log in to unmask] Subject: Selective Wave Soldering Status: I have been investigating selective wave soldering. Results to date have been less than desirable. The fixture is a huge heat sink, non-metal. The objective is to keep my SMD away from the wave while soldering a few through hole parts and eliminate my glue operation. The first fixture I tried held the CCA very high making it difficult to get successful soldering. Current machines are two super modified, nitro burning Hollis GBS Marks that have been modified with a High Mass Preheats, and modified Hot Air Knives with very flat CFM response curves. Also utilizing chip waves. I would appreciate any and all recommendations or experiences you would be willing to share. Thanks in advance. Ron From Hollis Land. --- End Included Message ---