Ralph Thanks for your inputs. I should have been more explicit. The laminate voids are definately in the pre-preg. The usually around the pad on the N-1 layer. Some have shown on other layers throughout the stack-ups but primarily N-1. If we have laminate voids usually is after solder float, some in as-built. Stack-ups vary on the board type but the anamoly is random. We dessicate our prepreg in nitrogen cabinets prior to use but do not vacuum evacuate. We have never had this problem. Thanks ______________________________ Reply Separator _________________________________ Subject: Re: FWD>Laminate Voids Author: [log in to unmask] at esdigate Date: 5/24/96 11:51 AM _____________________________ Reply Separator _________________________________ Subject: FWD>Laminate Voids Author: [log in to unmask] at SMTPpost1 Date: 5/23/96 9:12 PM Mail*Link(r) SMTP FWD>Laminate Voids <[log in to unmask]> inquired about "laminate voids" with the following: >We are looking for some help with a processing anomaly which surfaced > ~ six months ago. We began to see laminate voids in our epoxy boards. >Polyimide does not seem to be affected. We have verified lamination >cycles, investigated layer clean, oxide thickness and pre-clean. >Solutions seem to remain random. We are running low on ideas. >Has anyone out there experienced the same problems? Solutions? Riston >residues? Conversion coatings? >From: [log in to unmask] You probably have volatiles absorbed (moisture or solvent(s)) in the base (core) material or in the prepreg. If you have subsurface voids, in your cross sections you should be able to tell if the voids are in the core or prepreg If the voids are in the core material, then it is a supplier problem. If the voids are in the pregreg layers of the printed board then it can be either a core or prepreg material problem. In both cases, volatilize-out the materials prior to lamination using some form of desiccation such as heat and/or vacuum. If the voids are surface and you are foil laminating, you most probably have volitles in the prepreg and need to desiccate as above. Ralph Hersey e-mail: [log in to unmask]