Greetings, Does anyone have a good procedure for removing a warp/twist from a pcb? I am dealing with a .093 thick assembly that is 7 inches by 20 inches. The board currenly has smt components placed and soldered (topside only) but, the through hole components have not yet been mounted/soldered. I have tried heating the board and letting it cool while applying weight, that did not do the job. Any suggestions ? please respond. Thanks, [log in to unmask]