If it's too late to get 100% solder on this board, one possible solution could be addressed in design. I wonder if your designers use thermal pads for GND/PWR connections! I've had similar problems with an 11X11" board until we used thermal pads vs. direct connections to the layer. We had three layers of GND and we could never achieve the 100% flow. Good luck, bilal ______________________________ Reply Separator _________________________________ Subject: ASSM: Top fillet formation Author: [log in to unmask] at SMTPGATE Date: 12/20/96 6:34 PM Hello Technetters, I need some advises. I have a 6- layers board. I try to wave solder it, the solder at the ground point is not able to flow up to the top side of the board, in fact, it doesn't flow above 75%. We have tried using a solder-iron and set to temperature to 450 deg. cel. and hopefully able to force the solder through the PTH. Too bad, it didn't work anyway and it in fact has caused some lifted pads. We use full blow Nitrogeneous wave-solder machine, and the flux we use is only 1.2% solid content. And if the preheat temperature set to high, the flux gets degraded before it even reaches the wave.. I would like to know if anyone could advise me how wave-solder such a board with a great heavy thermal mass. Thanks in Advance.. =-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-==-=-=-=-=-=-=-=-=-=-==-=-=-=-=. / Kong Hui Poh / / Techgate / / - The Technological Gateway - / / Email Add: [log in to unmask] / / / / Fax Number: (65) 842 0318 / *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************