Me,too. Toru Koizumi [log in to unmask] ___________________________________ 返信 _______________________________________ 件名: re: open/short problem in fine line manufacturing 送信者: [log in to unmask] at ccs 日付: 96/12/13 12:11 I agree with Mr.Moody. Motoyo Wajima General Purpose Computer Division Hitachi,Ltd.(JAPAN) <[log in to unmask]> (Josh Moody) さんは書きました: >Can you be more specific, I think everyone experiences an increased > defect rate at finer lines and spaces. Can you tell us what type of > resist you are using? What is the surface prep prior to DF lamination? > Are you seeing alot of resist chips in your developer or etcher? >Are you catching the defect at AOI or Test? Are you pattern plating or >panel plating? What type of stripper are you using? Please answer > these questions first, then maybe this forum can you give some help. > >Regards, >Josh Moody >Merix Corp. > >*************************************************************************** >* TechNet mail list is provided as a service by IPC using SmartList v3.05 * >************************************************************************* ** >* To unsubscribe from this list at any time, send a message to: * >* [log in to unmask] with <subject: unsubscribe> and no text. * >********************************************************************** ***** >* If you are having a problem with the IPC TechNet forum please contact * >* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at sklydm@ ipc.org * >************************************************************ *************** > > *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * ************************************************************************* ** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * ********************************************************************** ***** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at sklydm@ ipc.org * ************************************************************ *************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************