In a message dated 96-12-08 20:46:52 EST, you write: >I'd like to hold a narrow etch rate window with fewer bath changes. > > Likely the only way to do this is with a color controlled feed and bleed apparatus. Tell us where your microetch is in the process, and if it is spray or immersion, and there may be some other ideas. Best regards, Rudy Sedlak RD Chemical Company *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************