Technetters: We have been using a 196 pin plastic QFP for some time now, but are in the process of replacing that package with a MQUAD 196pin package. I know that the MQUAD (Olin/Alphatec) package has been out there for quite some time now. However, I am wondering if there are any manufacturabilty issues that we should be aware of with the MQUAD package. Thank you ________________________________________________ Sanjay Rajan RF Communications Division Harris Corporation Product Design Engineering 1680 University Avenue Phone: (716) 242-3923 Rochester, NY 14610 Fax: (716) 242-3174 ________________________________________________ *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * ***************************************************************************